Type of Defect:  Sink mark

Cause Countermeasure
Caused by the shrinkage from slow cooling of thick wall section (unsuitable wall thickness) Reduce thickness deviation
Insufficient injection pressure Increase injection pressure
Insufficient shot capacity Increase shot capacity
Mold temperature is too high or insufficient cooling Increase cooling time if mold temperature is suitable
Insufficient pressure maintained Extend holding time
Insufficient gate dimension Increase gate dimension, especially thickness