Type of Defect: Al layer defect (2/2)
Description: Discoloration or Crack of the aluminium layer caused by chemical reaction (as time elapse)
Observation Method: Visible by the human eye
Recommendation Upon Observation:
Other Evaluation Method:
 
Cause Countermeasure
Chemical attack Adjust Al layer thickness (too thin)
Chemical attack Choose appropriate coating materials (ex. Pot life, contamination)
Humidity Adjust Al layer thickness (too thin)
Humidity Adjust coating layer thickness (too thin)
Humidity Adjust sputtering condition (ex. Vacuum level)
Humidity Choose appropriate coating materials (ex. Pot life, contamination)