Type of Defect: |
Rough Center Hole |
|
Description: |
Rough center hole |
|
Observation Method: |
|
|
Recommendation Upon Observation: |
|
|
Other Evaluation Method: |
|
|
|
|
Cause |
Countermeasure |
| Insufficient punching condition |
Adjust puncher temperature (too low) |
|
Insufficient punching condition |
Adjust punching condition (too late in usual) |
| Insufficient punching condition |
Adjust sprue bush temperature (too low) |
|
Insufficient punching condition |
Repair puncher |