Type of Defect: |
Silver streak (2/2) |
|
Description: |
White (or silver) streak running on the surface of the substrate along the flow of material |
|
Observation Method: |
Visible by the human eye / silvery scratch-like or hair-like streaks |
|
Recommendation Upon Observation: |
Better visibility under polarized light |
|
Other Evaluation Method: |
|
|
|
|
Cause |
Countermeasure |
| Material degradation caused by overheating |
Adjust cylinder temperature (too high) |
|
Material degradation caused by overheating |
Adjust nozzle temperature (too high) |
| Material degradation caused by overheating |
Check cylinder temperature equipment |
|
Material degradation caused by overheating |
Check the nozzle temperature controller |