Type of Defect: |
Void (2/2) |
|
Description: |
Hole in the PC substrate caused by Hydrolysis (as time elapse) |
|
Observation Method: |
Visible with microscope |
|
Recommendation Upon Observation: |
Better visibility under polarized light / visible as bright speck |
|
Other Evaluation Method: |
|
|
|
|
Cause |
Countermeasure |
| Hydrolysis of PC Caused by Humidity |
Check airborne dirt, alkalic agents from air dryer of material drying system |
|
Hydrolysis of PC Caused by Humidity |
Check environment of depository for disc products (room temperature and humidity) |